The purpose of the Multipurpose annealing furnace is annealing and dry oxidation of different samples and resist pyrolysis. Annealling and resist pyrolysis can be done in vaccum or at atmospheric pressure, in a N<sub>2</sub>, H<sub>2</sub> or a mixture of the two gasses. | The purpose of the Multipurpose annealing furnace is annealing and dry oxidation of different samples and resist pyrolysis. Annealling and resist pyrolysis can be done in vaccum or at atmospheric pressure, in a N<sub>2</sub>, H<sub>2</sub> or a mixture of the two gasses. | ||
All process gasses (except purge nitrogen) are heated heated, before they are introduced into the furnace at the door side. | |||
Is is possible to change all quartz ware in the furnace (the furnace tube, the door sealing and the wafer boat). A the moment Danchip is has three different sets of quartz ware: | Is is possible to change all quartz ware in the furnace (the furnace tube, the door sealing and the wafer boat). A the moment Danchip is has three different sets of quartz ware: | ||
Revision as of 14:28, 9 September 2015
Feedback to this page: click here
Multipurpose annealing furnace
The ATV Furnace


The Multipurpose annealing furnace it made by the company ATV Technologie, and it was installed in the cleanroom in 2015.
The purpose of the Multipurpose annealing furnace is annealing and dry oxidation of different samples and resist pyrolysis. Annealling and resist pyrolysis can be done in vaccum or at atmospheric pressure, in a N2, H2 or a mixture of the two gasses.
All process gasses (except purge nitrogen) are heated heated, before they are introduced into the furnace at the door side.
Is is possible to change all quartz ware in the furnace (the furnace tube, the door sealing and the wafer boat). A the moment Danchip is has three different sets of quartz ware:
- Clean: Dedicated for clean samples that have been RCA cleaned
- Metal: Dedicated for different samples that cannot be RCA cleaned. Also samples with metals are allowed in the furnace, when this quartz set is mounted
- Resist pyrolysis: Dedicated for resist pyrolysis.
Please note that all new materials have to be approved by the Thin Film group (thinfilm@danchip.dtu.dk) before they are allowed in the furnace.
The furnace tube is heated by use on 12 long heaters situated along the furnace tube and two flat heaters situated in the ends of the furnace tube. The this way the temperature will be very uniform everywhere in the furnace tube. The heating can be done very fast, up to 30 oC/min. For atmospheric pressure processes the maximum temperature is 1100 oC, and for vacuum processes the maximum temperature is 1050 oC. Cooling is done (rather slowly) by use of cooling fans.
For resist pyrolysis, samples with different resist layers are heated up to maximum 1100 oC in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample. If oxygen from the air or from outgassing of the resist is present in the furnace, the resist layer will be removed, thus it is important to evacuate the furnace and flush it with nitrogen, before a high temperature for resist pyrolysis is obtained. Pyrolysis of a large amount of resist may also be a problem due to resist outgassing.
The user manual, technical information and contact information can be found in LabManager:
Furnace: Multipurpose annealing
Process information
- Oxidation: look at the Oxidation page
- Annealing: look at the Annealing page
- Results from the Multipurpose Anneal Furnace acceptance test
| Purpose |
| |
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate materials allowed |
|