# '''Thickness of resist''': In general, it is recommended to work with an aspect ratio of ~1, i.e. where the width of the pattern is of same size than the thickness of the resist. Furthermore, when you decide for the resist thickness, consider which transfer you need:
# '''Thickness of resist''': In general, it is recommended to work with an aspect ratio of ~1, i.e. where the width of the pattern is of same size than the thickness of the resist. Furthermore, when you decide for the resist thickness, consider which transfer you need:
#* For lift-off processes, we recommend resist thicknnesses ~5 times larger than the thickness of the metal to be lifted.
#* For lift-off processes, we recommend resist thicknnesses ~5 times larger than the thickness of the metal to be lifted.
#* For dry or wet etch processes, investiagte the etch rates in resist as this might limit the minimum thickness of your resist.
#* For dry or wet etch processes, investiagte the etch rate of resist in your process as this might limit the minimum thickness of your resist.
# '''Mask''': Design and order a photomask for your UV process. A detailed instruction on how to design and order a photomask can be found [[Specific_Process_Knowledge/Lithography/Pattern_Design_and_Mask_Fabrication#Mask_Fabrication|here]].
# '''Mask''': Design and order a photomask for your UV process. A detailed instruction on how to design and order a photomask can be found [[Specific_Process_Knowledge/Lithography/Pattern_Design_and_Mask_Fabrication#Mask_Fabrication|here]].
# '''Substrate pretreatment''': In many processes it is recommended to pretreat your wafer before spin-coating. In some spin-coaters, these pretreatment processes are included in the spin coating of resist. If you use either the '''RCD8, SSE or a manual spin coater''', you should book equipment for pretreatment prior to spin  coating.
# '''Substrate pretreatment''': In many processes it is recommended to pretreat your wafer before spin-coating. In some spin-coaters, these pretreatment processes are included in the spin coating of resist. If you use either the '''RCD8, SSE or a manual spin coater''', you should book equipment for pretreatment prior to spin  coating.