Wet Silicon Oxide Etch (BHF and SIO Etch (wetting agent))

Silicon oxide can be etched using HF. At Danchip it is mainly used in a buffered version BHF (premixed). The BHF has a more stabil etch rate and has a high selectivty of oxide compared to photoresist which makes photoresist a good masking material for the oxide etch. However etching down to a silicon surface BHF leaves the siliocn surface slightly more rough than a pure HF solution.
SIO etch (BHF with wetting agent) can also be used for etching silicon oxide. This is mainly for etching small holes (~<?)
Silicon oxide etch data
| BHF | 5% HF | SIO | |
|---|---|---|---|
| General description |
Etching of silicon oxide with a stabil etch rate |
Mainly for removing native oxide |
. |
| Chemical solution | 6.5% HF and 30-40% NHF | 5% HF | BHF with wetting agent |
| Process temperature | Room temperature | Room temperature | Room temperature |
| Possible masking materials |
|
|
|
| Etch rate |
|
|
|
| Selectivity RSi3N4 / RSiO2 | ~21 | <21 | |
| Batch size |
1-25 wafers at a time |
1-25 wafer at a time | |
| Size of substrate |
2-6" wafers |
2-6" wafers | |
| Allowed materials |
|
|