Image:IBE 30min -Cr1.jpg |30min etch with 100nm Cr mask
Image:IBE 30min -Cr1.jpg |30min etch with 100nm Cr mask, used recipe BGHE blazed gratings with CHF3
Image:after IBE 45min_A_34.jpg |45min etch with 100nm Cr mask  
Image:after IBE 45min_A_34.jpg |45min etch with 100nm Cr mask, used recipe BGHE blazed gratings with CHF3
Image:Edge_1.jpg|20min etch with Krf resist, all resist is gone
Image:Edge_1.jpg|20min etch with Krf resist, all resist is gone, used recipe BGHE blazed gratings
Image:15min+30min5.jpg|15+30min etch with 50nm Cr mask
Image:15min+30min5.jpg|15+30min etch with 50nm Cr mask, used recipe BGHE blazed gratings with CHF3


</gallery>