Specific Process Knowledge/Wafer cleaning/7-up & Piranha: Difference between revisions
New page: {| border="2" cellspacing="0" cellpadding="4" align="left" ! ! 7-up ! Piranha |- |'''General description''' | Etch of pure Gold with or without photoresist mask. | Etch of pure Gold (as ... |
No edit summary |
||
Line 1: | Line 1: | ||
==Etching of Titanium== | |||
Etching of Titanium is done wet at Danchip. We have two solutions for titanium etching: | |||
{| border="2" cellspacing="0" cellpadding="4" align="left" | {| border="2" cellspacing="0" cellpadding="4" align="left" | ||
! | ! |
Revision as of 15:11, 14 February 2008
Etching of Titanium
Etching of Titanium is done wet at Danchip. We have two solutions for titanium etching:
7-up | Piranha | |
---|---|---|
General description |
Etch of pure Gold with or without photoresist mask. |
Etch of pure Gold (as stripper). |
Chemical solution | KJ:J:HO (100g:25g:500ml) | HCl:HNO (3:1) |
Process temperature | 20 oC | 20 oC |
Possible masking materials |
Photoresist (1.5 µm AZ5214E) |
Unmasked - used as a stripper |
Etch rate |
~100 nm/min |
~(??) nm/min - fast etch |
Batch size |
1-5 4" wafers at a time |
1-5 4" wafer at a time |
Size of substrate |
2-6" wafers |
2-6" wafers |