*[[/MVD|MVD]] - ''Molecular Vapor Deposition'' | *[[/MVD|MVD]] - ''Molecular Vapor Deposition'' | ||
*[[/Electroplating-Ni|Electroplating-Ni]] - ''Electrochemical deposition of nickel'' | *[[/Electroplating-Ni|Electroplating-Ni]] - ''Electrochemical deposition of nickel'' | ||
*MOCVD - Epitaxial growth - ''Ask the department of photonics if you are interested: | *MOCVD - Epitaxial growth - ''Ask the department of photonics if you are interested: [mailto:esem@fotonik.dtu.dk Elizaveta Semenova] or [mailto:kryv@fotonok.dtu.dk Kresten Yvind]'' | ||
|- | |- | ||
|} | |} | ||
Revision as of 15:30, 10 December 2014
Feedback to this page: click here
Choose material to deposit
| Dielectrica | Semicondutors | Metals | Alloys | Transparent conductive oxides | Polymers |
|
Silicon Nitride - and oxynitride |
Aluminium |
TiW alloy (10%/90% by weight) |
SU8 |
Choose deposition equipment
| PVD | LPCVD | PECVD | ALD | Coaters | Others
|
|
|
|
|
See the Lithography/Coaters page for coating polymers |
|