Line 90: Line 90:
*'''DCH 100mm PEB60s@110C+SP60s'''
*'''DCH 100mm PEB60s@110C+SP60s'''
A combination of the 'DCH PEB 110C 60s' post-exposure bake and the 'DCH 100mm SP 60s' development.
A combination of the 'DCH PEB 110C 60s' post-exposure bake and the 'DCH 100mm SP 60s' development.
*'''DCH 100mm PEB60s@110C+SP30s'''
A combination of the 'DCH PEB 110C 60s' post-exposure bake and the 'DCH 100mm SP 30s' development.