; Equations: | ; Equations: | ||
: Determines what to do with the data from each region. Press Insert and select 'Region Equation'. Here, select | : Determines what to do with the data from each region. Press Insert and select 'Region Equation'. Here, select | ||
* Appropriate names and colors as with regions. | |||
* Spectrum: Only one choice | |||
* Region according to name | |||
* Operation: Typically one will choose 'Max' to find the peak within each region, see image below. Other possibilities are Sum, Average, Min or Median. | |||