*Isotropic | *Isotropic | ||
|- | |- | ||
|style="background:LightGrey; color:black"|See more [[/BHF etch rates|etch rates]] | |style="background:LightGrey; color:black"|Etch rates | ||
See more [[/BHF etch rates|etch rates]] | |||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
*Wet thermal oxide:75-80nm/min | *Wet thermal oxide:75-80nm/min | ||