Wet Silicon Nitride Etch
Wet Etching of silicon nitride is done in a dedicated laminar flow bench with an integrated quartz tank (Tiger Tank - TT-4). The quartz tank can take up to one 6" wafer carrier. The flow bench is placed in cleanroom 4.
The etch solution is initially 85 wt% HPO which is heated up to the boiling temperature - ca. 157 oC. Water is allowed to boil off thus raising the concentration and the boiling temperature of the solution until a boiling temperature of 180 oC is reached. Thereafter, the wafers are submerged into the bath and the water-cooled lid is closed to maintain the concentration and the boiling temperature. In some cases a lower boiling temperature is chosen - typically 160 oC - which lowers the etch rate and improves the selectivity RSi3N4 / RSiO2
Nitride etch - key facts
| Nitride etch @ 180 oC | Nitride etch @ 160 oC | |
|---|---|---|
| General description |
Etch of pure Gold |
Etch of pure Gold |
| Chemical solution | KJ:J:HO (100g:25g:500ml) | HCl:HNO (3:1) |
| Process temperature | 20 oC | 20 oC |
| Possible masking materials: |
Photoresist (1.5 µm AZ5214E) |
Photoresist (1.5 µm AZ5214E) |
| Etch rate |
~100 nm/min (Pure Al) |
~(??) nm/min |
| Batch size |
1-25 wafers at a time |
1-25 wafer at a time |
| Size of substrate |
2-6" wafers |
2-6" wafers |