Specific Process Knowledge/Lithography/CSAR: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 28: | Line 28: | ||
|[[Specific_Process_Knowledge/Lithography/Coaters#Manual Spinner 1|Manual Spinner 1 (Laurell)]], [[Specific_Process_Knowledge/Lithography/Coaters#Spin_coater:_Manual_Labspin|Spin Coater Labspin]] | |[[Specific_Process_Knowledge/Lithography/Coaters#Manual Spinner 1|Manual Spinner 1 (Laurell)]], [[Specific_Process_Knowledge/Lithography/Coaters#Spin_coater:_Manual_Labspin|Spin Coater Labspin]] | ||
|X AR 600-54/6, MIBK:IPA | |X AR 600-54/6, MIBK:IPA | ||
|IPA | |IPA, H2O | ||
|1165 Remover | |1165 Remover | ||
|[[media:Process_Flow_CSAR.docx|Process_Flow_CSAR.docx]] | |[[media:Process_Flow_CSAR.docx|Process_Flow_CSAR.docx]] | ||