{| border="1" cellspacing="2" cellpadding="2"  
{| border="1" cellspacing="2" cellpadding="2"  
![[image:140618_FluenceVSrepRate_1064nm_IPG.jpg|500x500px|thumb|center|Fluence result for IR wavelength (IPG 1064nm, F255mm)]]
![[image:140618_FluenceVSrepRate_1064nm_IPG.jpg|500x500px|thumb|center|Fluence result for IR wavelength (IPG 1064nm, F255mm). The fluence at 100% and 10kHz must be expected around 25J/cm2]]


|}
|}