Specific Process Knowledge/Lithography/CSAR: Difference between revisions
Appearance
| Line 297: | Line 297: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
|Spin Coat | |Spin Coat | ||
|6000 rpm, 4000 1/s2, 60 sec, Softbake 1 min @ 150 degC | |6000 rpm, 4000 1/s2, 60 sec, Softbake 1 min @ 150 degC, thickness ~140nm | ||
|- | |- | ||