# It is crucial to have your pattern ready in GDSII format. Check your GDS-file by importing it in e.g. <span class="plainlinks">[http://www.wieweb.com/ns6/index.html CleWin]</span> or L-edit. In order to reach the files from the computers inside the cleanroom it is recommended to either dropbox them or send them per email to yourself.  
# It is crucial to have your pattern ready in GDSII format. Check your GDS-file by importing it in e.g. <span class="plainlinks">[http://www.wieweb.com/ns6/index.html CleWin]</span> or L-edit. In order to reach the files from the computers inside the cleanroom it is recommended to either dropbox them or send them per email to yourself.  
# Create sdf and jdf-files; read the sdf and jdf-file manual from technical documents found [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=292 here]
# Create sdf and jdf-files; read the sdf and jdf-file manual from technical documents found [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=292 here]
# Assist a fully trained colleague of yours when she or he e-beam writes, gather as much knowledge about your e-beam run, i.e. which e-beam current, aperture and dose to use, which shot pitch (e.g. SHOT A,10).  
# Assist a fully trained colleague of yours when she or he e-beam writes, gather as much knowledge about your e-beam run, i.e. which e-beam current, aperture and dose to use, which shot pitch (e.g. SHOT A,10).  
# Study the logbook for the e-beam writer: sheet 1 gives you an overview of which condition files (currents and apertures) have been in use recently by which user on which type of resist. On sheet 2 in this logbook you can find a writing time estimation program.
# Study the logbook for the e-beam writer: sheet 1 gives you an overview of which condition files (currents and apertures) have been in use recently by which user on which type of resist. On sheet 2 in this logbook you can find a writing time estimation program.
# Study all 3 manuals for the machine, they can be found [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=292 here]
# Study all 3 manuals for the machine, they can be found [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=292 here]