==KOH etch - ''Anisotropic silicon etch''==
==KOH etch - ''Anisotropic silicon etch''==
[[Image:KOH_4tommer.jpg|300x399px|thumb|KOH etch for 4" wafers: positioned in cleanroom 3]]
[[Image:KOH_4tommer.jpg|300x399px|thumb|KOH etch for 4" wafers: positioned in cleanroom 3]]
KOH belongs to the family of anisotropic Si-etchants based on aqueous alkaline solutions. The anisotropy stems from the different etch rates in different crystal directions.
KOH belongs to the family of anisotropic Si-etchants based on aqueous alkaline solutions. The anisotropy stems from the different etch rates in different crystal directions. The {111}-planes are almost inert whereas the etch rates of e.g. {100}- and {110}-planes are several orders of magnitude faster.
 
At Danchip we use as a standard a 28 wt% KOH.

Revision as of 11:31, 28 January 2008

KOH etch - Anisotropic silicon etch

KOH etch for 4" wafers: positioned in cleanroom 3

KOH belongs to the family of anisotropic Si-etchants based on aqueous alkaline solutions. The anisotropy stems from the different etch rates in different crystal directions. The {111}-planes are almost inert whereas the etch rates of e.g. {100}- and {110}-planes are several orders of magnitude faster.

At Danchip we use as a standard a 28 wt% KOH.