: <math>Fluence = \frac{E_{pulse}}{S}\,</math>
: <math>Fluence = \frac{E_{pulse}}{A}\,</math>


The theoretical spot sizes (<math>S</math>) can be found [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Spot size and optics|here]]
The theoretical spot sizes (<math>A</math>) can determinate with the min spot size set [[Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/Spot size and optics|here]]


== Fluence results measurement==
== Fluence results measurement==

Revision as of 16:18, 26 May 2014

Fluence definition

The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (Epulse) per surface unit (S) and it is given in J/cm2.


The function Epulse is defined as :


Epulse=P‾f

Where P‾ (average power) is measured with the laser sensor power measurement (see manual,section 5.3) and the repetion rate (f) is set in the parameter file under " laser frequency".

The fluence is therefore determinated as such :


Fluence=EpulseA

The theoretical spot sizes (A) can determinate with the min spot size set here

Fluence results measurement

Fluence result for IR wavelength (1064nm, F255mm)
Fluence result for green wavelength (532nm, F255mm)
Fluence result for UV wavelength (355nm, F255mm)