'''(1)''' Temperature of mixture is ~22 C (no heating during etch). data obtained using magnetic stirring with sample on flat basket. '''(2)''' Refrigerated H2O used during mixture of etch, and mixture kept at 17 C during etch. '''(3)''' 10:2:30 gives smoother etch than 10:2:60.