CSAR | CSAR | ||
{|border="1" cellspacing="0" cellpadding="3" style="text-align:left;" | |||
|- | |||
|- | |||
|-style="background:LightGrey; color:black" | |||
!colspan="3"|Spin Coat of AllResist SX 6200/2, TIGRE, 09-04-2014 | |||
|- | |||
|- | |||
|-style="background:silver; color:black" | |||
!Spin Coater | |||
!Process Parameters | |||
!Comments | |||
|- | |||
|- | |||
|-style="background:silver; color:black" | |||
|Spin Coater Manual, LabSpin, A-5 | |||
|60 sec at various spin speed. Acceleration 4000 s-2, softbake 5 min at 150 deg Celcius | |||
|Resist poured directly from bottle | |||
|- | |||
|} | |||