==KOH etch - ''Anisotropic silicon etch''==
==KOH etch - ''Anisotropic silicon etch''==
[[Image:KOH_4tommer.jpg|300x399px|thumb|KOH etch for 4" wafers: positioned in cleanroom 3]]
[[Image:KOH_4tommer.jpg|300x399px|thumb|KOH etch for 4" wafers: positioned in cleanroom 3]]
KOH is an anisotropic Si-etch.