We have observed that using automatic developing we can decrease the exposure dose for resolve the 250nm pillors structures comparing to dose needed for resolve the line the same size. | We have observed that using automatic developing we can decrease the exposure dose for resolve the 250nm pillors structures comparing to dose needed for resolve the line the same size. | ||
[[Image: | [[Image:140_250_NM_TILT22.TIF|300×300px|right|thumb|The SEM picture of 250nm pillors and lines. Exposure dose is 140 J/m2.]] | ||