Jump to content

Specific Process Knowledge/Back-end processing/Wire Bonder: Difference between revisions

From LabAdviser
BGE (talk | contribs)
No edit summary
Jehan (talk | contribs)
No edit summary
Line 1: Line 1:
==TPT Wire Bonder==
==TPT Wire Bonder==


[[Image:TPTWireBonder.jpg|300x300px|thumb|TPT Wire Bonder Building 346, 2nd floor]]
[[Image:TPTWireBonder.jpg|300x300px|thumb|TPT Wire Bonder, Packlab, Building 347, 2nd floor]]
[[Image:TPTwirebonder_wedge_ball.jpg|300x300px|thumb|Wire bondings: Left: wedge bonding - Right: ball bonding]]
[[Image:TPTwirebonder_wedge_ball.jpg|300x300px|thumb|Wire bondings: Left: wedge bonding - Right: ball bonding]]



Revision as of 10:02, 29 September 2011

TPT Wire Bonder

Error creating thumbnail: File missing
TPT Wire Bonder, Packlab, Building 347, 2nd floor
Wire bondings: Left: wedge bonding - Right: ball bonding

The TPT Wire Bonder is a new machine bought i 2007. Wire bonding is a method of making interconnections between a microchip and other electronics as part of semiconductor device fabrication. The TPT-H05 is a manuel wire bonder.


Please be aware that the bonder only is operated by Danchip personal.



Wedge Bonding

  • Gold wire 25 µm wire.
  • Aluminium wire 25 µm wire.
  • Min. bonding area 200 µm.


Ball Bonding

Ball bonding gives free choice of bonding direction. First bond forms a small ball and second bond is a wedge bond.

  • Gold only 25 µm wire.
  • Min. bonding pad 300 µm.
  • Sample withstand heating to 120 oC.