==Etching of Gold==
==Etching of Gold==
Etching of Gold is done wet at Danchip making your own set up in the fumehood. We have two different solutions:
Etching of Gold is done wet at Danchip making your own set up in a beaker in the fumehood. We have two different solutions:


# Iodine etch: KI:I<math>_2</math>:H<math>_2</math>O - 400g:100g:400ml?
# Iodine etch: KI:I<math>_2</math>:H<math>_2</math>O - 400g:100g:400ml?