Etching of Gold is done wet at Danchip making your own set up in the fumehood. We have two different solutions: | Etching of Gold is done wet at Danchip making your own set up in the fumehood. We have two different solutions: | ||
# KI:I<math>_2</math>:H<math>_2</math>O - 400g:100g:400ml? | # Iodine etch: KI:I<math>_2</math>:H<math>_2</math>O - 400g:100g:400ml? | ||
# HNO<math>_3</math>:HCl - 1:3 | # HNO<math>_3</math>:HCl - 1:3 | ||