Specific Process Knowledge/Etch/Etching of Gold: Difference between revisions
Line 40: | Line 40: | ||
~100 nm/min (Pure Al) | ~100 nm/min (Pure Al) | ||
| | | | ||
~ | ~(??) nm/min | ||
|- | |- | ||
|Batch size | |Batch size |
Revision as of 15:05, 18 January 2008
Etching of Gold
Etching of Gold is done wet at Danchip. We have two different solutions:
- KI:I:HO - 400g:100g:400ml?
- HNO:HCl - 1:3
Comparing the two solutions
Iodine based gold etch | Aqua Regia (Kongevand) | |
---|---|---|
General description |
Etch of pure Gold |
Etch of pure Gold |
Chemical solution | KJ:J:HO 100g:25g:500ml | H:HO |
Process temperature | 20 oC | 20 oC |
Possible masking materials: |
Photoresist (1.5 µm AZ5214E) |
Photoresist (1.5 µm AZ5214E) |
Etch rate |
~100 nm/min (Pure Al) |
~(??) nm/min |
Batch size |
1-25 wafers at a time |
1-25 wafer at a time |
Size of substrate |
4" wafers |
4" wafers |
Allowed materials |
|
|