'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Annealing click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Annealing click here]''' | ||
Revision as of 15:31, 19 March 2014
Feedback to this page: click here
Annealing
At Danchip we have three furnaces and an RTP for annealing: C1, C3, Noble furnace and Jipelec RTP. Annealing normally takes place in an N2 atmosphere. PECVD PBSG is annealed in an wet atmosphere which will also oxidize the silicon substrate.
The furnace for oxidation are made so a 20 minutes N2 annealing step is include and it is not normally necessary to make one more annealing of the wafers.
Comparison of the annealing furnaces
| General description | Annealing of 6" wafers. Annealing of wafers from the LPCVD furnaces and PECVD1. | Annealing of wafers from EVG-NIL, PECVD3 and wafers with aluminum. | Annealing of almost materials on silicon wafer. | Rapid thermal annealing |
|---|---|---|---|---|
| Annealing gas |
|
|
|
|
| Process temperature |
|
|
|
|
| Substrate and Batch size |
|
|
|
|
| Allowed materials |
|
|
|
|