Jump to content

Specific Process Knowledge/Etch/Etching of Gold: Difference between revisions

Line 23: Line 23:
|-
|-
|Process temperature
|Process temperature
|50 <sup>o</sup>C
|20 <sup>o</sup>C


|20 <sup>o</sup>C
|20 <sup>o</sup>C