==Etching of Chromium==
==Etching of Chromium==
Etching of chromium is done wet at Danchip. We have two solution for this:
Etching of chromium is done wet at Danchip making your own set up in a beaker in the fumehood. We have two solution for this:


# HNO<math>_3</math>:H<math>_2</math>O:cerisulphate  - 90ml:1200ml:15g
# HNO<math>_3</math>:H<math>_2</math>O:cerisulphate  - 90ml:1200ml:15g - standard at Danchip
# Commercial chromium etch
# Commercial chromium etch