Deposition of TiW alloy can take place in the Wordentec. '''Observe:''' ''right now we don´t have a TiW target for Wordentec, please contact thinfilm@danchip.dtu.dk if you are interested in depositing TiW.''
Deposition of TiW alloy can take place in the Wordentec.  




'''Observe:''' ''right now we don´t have a TiW target for Wordentec, please contact thinfilm@danchip.dtu.dk if you are interested in depositing TiW.''


{| border="1" cellspacing="0" cellpadding="4"  
{| border="1" cellspacing="0" cellpadding="4"  

Revision as of 16:01, 17 March 2014

Feedback to this page: click here


Deposition of TiW alloy can take place in the Wordentec.


Observe: right now we don´t have a TiW target for Wordentec, please contact thinfilm@danchip.dtu.dk if you are interested in depositing TiW.

Sputter deposition (Wordentec)
Batch size
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Pre-clean RF Ar clean
Layer thickness .
Allowed substrates
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
Allowed materials
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
Deposition rate Depending on process parameters, see here.
Comments TiW alloy: 10%/90% by weight


Deposited rates

This is done by a sputtering process. Process parameters (argon pressure and effect) can be varied, the surface roughness and the deposition rate (see here) and may change with these settings.


Deposited film characteristics

AFM pictures show how the surface roughness is dependent of the process parameters, this can be seen here.