* Metals  
* Metals  
|
|
NiV (75 - 100 nm recommended)
* NiV (75 - 100 nm recommended)
Ti (5 nm) + Au (75-100 nm recommended)
* Ti (5 nm) + Au (75-100 nm recommended)
Cr (5 nm) + Au (75-100 nm recommended)
* Cr (5 nm) + Au (75-100 nm recommended)
Cr
* Cr
TiW
* TiW
|-
|-
|-
|-