Specific Process Knowledge/Wafer cleaning/7-up & Piranha: Difference between revisions

Kabi (talk | contribs)
Kabi (talk | contribs)
No edit summary
Line 9: Line 9:
[[Image:7-up_6inch.jpg|300x300px|right|thumb|7-up 6" in cleanroom D3. <br\> -Up to 25 wafers of 4" or 6" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]
[[Image:7-up_6inch.jpg|300x300px|right|thumb|7-up 6" in cleanroom D3. <br\> -Up to 25 wafers of 4" or 6" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]
[[Image:7-up_Mask.jpg|300x300px|right|thumb|7-up for masks and glass wafers positioned in cleanroom D3:<br\> -Up to 25 glass wafers of 4" at a time or 4 masks.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi, glass, chromium]]
[[Image:7-up_Mask.jpg|300x300px|right|thumb|7-up for masks and glass wafers positioned in cleanroom D3:<br\> -Up to 25 glass wafers of 4" at a time or 4 masks.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi, glass, chromium]]
[[Image:7-up_RR3.jpg|300x300px|right|thumb|7-up 4": positioned in cleanroom C1<br\> -Up to 19 wafers of 4" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]
!![[Image:7-up_RR3.jpg|300x300px|right|thumb|7-up 4": positioned in cleanroom C1<br\> -Up to 19 wafers of 4" at a time.<br\> -Materials allowed: Silicon, Silicon oxide, Silicon nitride, PolySi]]!!


===Comparing data for "7-up" and Piranha===
===Comparing data for "7-up" and Piranha===