Specific Process Knowledge/Wafer cleaning: Difference between revisions
Appearance
| Line 42: | Line 42: | ||
|Mandatory prior furnace processes | |Mandatory prior furnace processes | ||
|When needed and always after KOH etch and Nitride etch in Phosphoric acid | |When needed and always after KOH etch and Nitride etch in Phosphoric acid | ||
|Optional | |Optional during RCA cleaning | ||
|Cleaning before wafer bonding | |Cleaning before wafer bonding | ||
|Cleaning very dirty items that enters the cleanroom. Should be followed by a piranha clean. | |Cleaning very dirty items that enters the cleanroom. Should be followed by a piranha clean. | ||
Revision as of 11:56, 3 March 2014
Feedback to this page: click here
Clean with:
- RCA - Two step process to remove organics and metals
- 7-up & Piranha - Removes organics and alkali ions
- 5% HF - Removing native oxide
- IMEC - Cleaning before fusion bonding
- Soap Sonic - Cleaning of "dirty" wafers when entering the cleanroom
Section under construction
Comparison of Wafer Cleaning Methods
| RCA | 7-up & Piranha | 5% HF | IMEC | Soap Sonic | |
|---|---|---|---|---|---|
| Generel description | Two step process to remove organics and metals | Removes organics and alkali ions | Removing native oxide | Cleaning before wafer bonding | Removing dust and particles |
| Purpose | Mandatory prior furnace processes | When needed and always after KOH etch and Nitride etch in Phosphoric acid | Optional during RCA cleaning | Cleaning before wafer bonding | Cleaning very dirty items that enters the cleanroom. Should be followed by a piranha clean. |
| Substrate size |
|
|
|
|
|
| Allowed materials |
|
|
|
|
|