The spray coater at Danchip is located in Cleanroom C-1. The machine is an ExactaCoat from Sono-tek which can be fitted with one of three different nozzles depending on the nature of the spray coating tasks at hand. The three different nozzles (Impact, AccuMist and Vortex) are optimized for different applications such as spray coating of large areas (e.g. entire wafers), smaller areas (e.g. wafer pieces or other small samples) or already structured samples that cannot be coated uniformly by spin coating. All nozzles use an ultrasonic tranducer for atomizing the solution to be spray coated. It is therefore a prerequisite that all components are compatible with this process. This is the case with most substances, although process parameters may need optimization to give satisfactory results.
The spray coater at Danchip is located in Cleanroom C-1. The machine is an ExactaCoat from Sono-tek which can be fitted with one of three different nozzles depending on the nature of the spray coating tasks at hand. The three different nozzles (Impact, AccuMist and Vortex) are optimized for different applications such as spray coating of large areas (e.g. entire wafers), smaller areas (e.g. wafer pieces or other small samples) or already structured samples that cannot be coated uniformly by spin coating. All nozzles use an ultrasonic tranducer for atomizing the solution to be spray coated. It is therefore a prerequisite that all components are compatible with this process. This is the case with most substances, although process parameters may need optimization to give satisfactory results.


Practically any sample that will fit inside the spray coater can be processed. Spray patterns are easily programmed either using predefined spray patterns (1D line, 2D rectangles/circles/meanders/spirals or custom 3D spray patterns).
Practically any sample that will fit inside the spray coater can be processed. Spray patterns are easily programmed either using predefined spray patterns (1D line, 2D rectangles/circles/meanders/spirals) or custom 3D spray patterns.


The spray coating process as well as major features of the three nozzles are described into more detail in the manual which can be found via the Equipment Info page in LabManager. It can be found be clicking Equipment -> Info or by using the direct link below. Then follow the 'User Manual' link.
The spray coating process as well as major features of the three nozzles are described into more detail in the manual which can be found via the Equipment Info page in LabManager. It can be found be clicking Equipment -> Info or by using the direct link below. Then follow the 'User Manual' link.

Revision as of 11:44, 6 May 2014

Feedback to this page: click here

Spray Coater

Spray Coater in Cleanroom C-1

The spray coater at Danchip is located in Cleanroom C-1. The machine is an ExactaCoat from Sono-tek which can be fitted with one of three different nozzles depending on the nature of the spray coating tasks at hand. The three different nozzles (Impact, AccuMist and Vortex) are optimized for different applications such as spray coating of large areas (e.g. entire wafers), smaller areas (e.g. wafer pieces or other small samples) or already structured samples that cannot be coated uniformly by spin coating. All nozzles use an ultrasonic tranducer for atomizing the solution to be spray coated. It is therefore a prerequisite that all components are compatible with this process. This is the case with most substances, although process parameters may need optimization to give satisfactory results.

Practically any sample that will fit inside the spray coater can be processed. Spray patterns are easily programmed either using predefined spray patterns (1D line, 2D rectangles/circles/meanders/spirals) or custom 3D spray patterns.

The spray coating process as well as major features of the three nozzles are described into more detail in the manual which can be found via the Equipment Info page in LabManager. It can be found be clicking Equipment -> Info or by using the direct link below. Then follow the 'User Manual' link.

The user manual, user APV, technical information and contact information can be found in LabManger:

Spray coater in LabManager

Equipment performance and process related parameters

Equipment Spray Coater
Purpose
  • Spraying imprint resist
  • Spraying photoresist
  • Spraying of other solutions
Performance Substrate handling
  • Can handle almost any sample size and shape
Permanent media
  • No permanent media
Manual dispense option
  • Two syringe pumps
Process parameter range Solution viscosity
  • Range
Chemical properties
  • Must be non-toxic
  • Compatible with titanium
  • Resistant to ultrasonic atomization
Substrates Batch size
  • Any sample(s) that fit inside machine
Allowed materials
  • All chemicals to be spray coated must be approved specifically for spray coating
  • Any non-toxic, non-particulate and non-crosslinking material is likely to be approved