Wafers with metals or other materials, not allowed in the dedicated oxide etch baths, can be etched in the PP-bath positioned in the fume hood in cleanroom 2 or in a '''plastic''' beaker. | Wafers with metals or other materials, not allowed in the dedicated oxide etch baths, can be etched in the PP-bath positioned in the fume hood in cleanroom 2 or in a '''plastic''' beaker. | ||
'''The user manual for all HF/BHF baths, APV's and contact information can be found in LabManager | '''The user manual for all HF/BHF baths, APV's and contact information can be found in LabManager''' [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=64 by clicking here] | ||