Specific Process Knowledge/Etch/Wet Aluminium Etch: Difference between revisions
Appearance
| Line 7: | Line 7: | ||
# Pre-mixed etch solution: PES 77-19-04 at 20 <sup>o</sup>C | # Pre-mixed etch solution: PES 77-19-04 at 20 <sup>o</sup>C | ||
Both solutions are used in the Aluminium etch bath shown to the right. I must be written on which one is in. | Both solutions are used in the Aluminium etch bath shown to the right. I must be written on which one is in. Solution no. 1 is the most used solution for etchning oure aluminium. Solution no. 2 is primarily for etching aluminium mixed with a small percentage of silicon. | ||