Etching of Gold is done wet at Danchip. We have two different solutions:
Etching of Gold is done wet at Danchip. We have two different solutions:


# KI:I<math>_2</math>:H<math>_2</math>O<math>  400g:100g:400ml?
# KI:I<math>_2</math>:H<math>_2</math>O - 400g:100g:400ml?
# HNO<math>_3</math>:HCl 1:3
# HNO<math>_3</math>:HCl - 1:3