Specific Process Knowledge/Lithography: Difference between revisions
| Line 218: | Line 218: | ||
==[[Specific Process Knowledge/Lithography/DUVStepperLithography|DUV Stepper Lithography]]== | ==[[Specific Process Knowledge/Lithography/DUVStepperLithography|DUV Stepper Lithography]]== | ||
*[[Specific Process Knowledge/Lithography/DUVStepper#SÜSS Spinner-Stepper|SÜSS Spinner-Stepper]] | *[[Specific Process Knowledge/Lithography/DUVStepper#SÜSS Spinner-Stepper|SÜSS Spinner-Stepper]] | ||
*[[Specific Process Knowledge/Lithography/DUVStepper#Process information|Process information]] | **[[Specific Process Knowledge/Lithography/DUVStepper#Process information|Process information]] | ||
*[[Specific Process Knowledge/Lithography/DUVStepper#DUV Stepper FPA-3000EX4 from Canon|DUV Stepper FPA-3000EX4 from Canon]] | *[[Specific Process Knowledge/Lithography/DUVStepper#DUV Stepper FPA-3000EX4 from Canon|DUV Stepper FPA-3000EX4 from Canon]] | ||
*[[Specific Process Knowledge/Lithography/DUVStepper#Process information|Process information]] | **[[Specific Process Knowledge/Lithography/DUVStepper#Process information|Process information]] | ||
*[[Specific Process Knowledge/Lithography/DUVStepper#Overview of performance|Overview of performance]] | **[[Specific Process Knowledge/Lithography/DUVStepper#Overview of performance|Overview of performance]] | ||
==[[Specific Process Knowledge/Lithography/EBeamLithography|E-Beam Lithography]]== | ==[[Specific Process Knowledge/Lithography/EBeamLithography|E-Beam Lithography]]== | ||
Revision as of 15:33, 19 February 2014

Feedback to this page: click here
Mask Design
In order to realize your device you will need a way to draw the patterns that define the structures in the different layers on the wafer. This is done in a drawing tool for mask layout. The output is a file you send to a mask house, which in return supplies you with a number of photolithographic masks. Each mask is a glass plate with a chromium pattern that mimics a layer in your layout.
Please read more details here: Mask Design
Comparing lithography methods at DTU Danchip
| UV Lithography | DUV Stepper Lithography | E-beam Lithography | Nano Imprint Lithography |
2-Photon Polymerization Lithography | |
|---|---|---|---|---|---|
| Generel description | Pattern transfer via UltraViolet (UV) light | Pattern transfer via DeepUltraViolet (DUV) light | Pattern transfer via electron beam | Pattern transfer via hot embossing(HE) | Pattern transfer via direct writing |
| Pattern size range |
|
|
|
|
|
| Resist type |
|
|
|
|
|
| Resist thickness range |
~0.5µm to 20µm |
~50nm to 2µm |
~30nm to 0.5 µm |
~ 100nm to 2µm |
droplet |
| Typical exposure time |
2s-30s pr. wafer |
Process depended, depends on pattern, pattern area and dose |
Depends on dose, Q [µC/cm2], beam current, I [A], and pattern area, A [cm2]: t = Q*A/I |
Process depended, depends also on heating and cooling temperature rates |
Process depended, depends on pattern and dose |
| Substrate size |
|
|
We have cassettes that fit to
Only one cassette can be loaded at time |
|
|
| Allowed materials |
|
|
|
|
|