== BCB Curing Oven ==
== BCB Curing Oven ==
[[image:BCB oven.jpeg|350x350px|right|thumb|The BCB Curing Oven. Located in the III-V Lab]]
[[image:BCB oven.jpeg|350x350px|right|thumb|The BCB Curing Oven. Positioned in the A-5 room]]


The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of metals in a nitrogen atmosphere.
The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of metals in a nitrogen atmosphere.