Feedback to this page: click here
Die bonder (eutectic metal soldering)
The Cammax EDB80 Die bonder is for placing and soldering dies onto a package or substrate.
The user manuals, user APVs, technical information and contact information can be found in LabManager:

Process information
Flip-chip bonder (glue attachment)

Flip-chip Bonder in LabManager (not there yet)
Equipment | Die bonder | Flip-chip bonder | |
---|---|---|---|
Purpose |
|
| |
Performance |
|
| |
Substrates | Allowed materials |
|
|