=Depth profiling=
=Depth profiling=


[[Image:Stochiometry 20110510.JPG|425x425px|left|thumb|The composition of a NiCr as a function of film depth (etch time). The relationship between Cr and Ni is quite constant through the 70nm thick film. Measurements done with XPS-ThermoScientific. ]]
[[Image:Stochiometry 20110510.JPG|500x500px|left|thumb|The composition of a NiCr as a function of film depth (etch time). The relationship between Cr and Ni is quite constant through the 70nm thick film. Measurements done with XPS-ThermoScientific. ]]


The analysis is made on a chosen spot on the sample surface (chosen with the system camera). The technique is, as written above, very surface sensitive and probes only the top nanometers of the sample.  
The analysis is made on a chosen spot on the sample surface (chosen with the system camera). The technique is, as written above, very surface sensitive and probes only the top nanometers of the sample.  

Revision as of 17:04, 27 January 2014

Depth profiling

The composition of a NiCr as a function of film depth (etch time). The relationship between Cr and Ni is quite constant through the 70nm thick film. Measurements done with XPS-ThermoScientific.

The analysis is made on a chosen spot on the sample surface (chosen with the system camera). The technique is, as written above, very surface sensitive and probes only the top nanometers of the sample.

With the ion beam gun on the system an etch of the sample can be done. The system measures the desired spectrum, does an etch step and measures again. A series of etch cycles can be set up, measuring the composition of the sample at different depths (for example at different depth of a film).


Example: NiCr film

As an illustration, a figure to the left, shows an elemental analysis through a metallic film consisting of Ni and Cr. The metallic layer was about 70 nm thick, and the atomic percentage of Ni and Cr was measured through the layer.

In the graph, you see the atomic % as a function of etch depth, and it is possible to detect that the relationship between Ni and Cr is fairly constant through the metallic film.