Jump to content

Specific Process Knowledge/Characterization/Thickness Measurer: Difference between revisions

From LabAdviser
Pevo (talk | contribs)
Pevo (talk | contribs)
Line 35: Line 35:
Thickness measurer
Thickness measurer
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Wafer
*Wafer thickness
*Depths of larger grooves
*Depths of larger grooves
*Heigth of larger mesas
*Heigth of larger mesas
Line 44: Line 44:
Thickness resolution  
Thickness resolution  
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*>5 µm
*< 5 µm
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|
Process parameter range
|style="background:LightGrey; color:black"|
Process Temperature
|style="background:WhiteSmoke; color:black"|
*Room temperature
|-
|-
|style="background:LightGrey; color:black"|Process pressure
|style="background:LightGrey; color:black"|Process pressure
Line 66: Line 59:
| style="background:LightGrey; color:black"|Substrate materials allowed
| style="background:LightGrey; color:black"|Substrate materials allowed
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*No restriction.
*No restrictions
|-  
|-  
|}
|}

Revision as of 11:17, 15 January 2014

THIS PAGE IS UNDER CONSTRUCTION

Feedback to this page: click here

Thickness measurer

Digital Thickness Measurer. Positioned in cleanroom 4

The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.

Doing a KOH etch can it be helpful to ensure no over-etching by making a thickness measurement during the etching.

The user manual, technical information and contact information can be found in LabManager:

Thickness measurer

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result have to be within ± 0.005 mm. The QC is preformed ones a year.

Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer thickness
  • Depths of larger grooves
  • Heigth of larger mesas

Performance

Thickness resolution

  • < 5 µm
Process pressure
  • 1 atm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions