Specific Process Knowledge/Thermal Process/Furnace Noble: Difference between revisions
Appearance
| Line 6: | Line 6: | ||
The Noble Furnace is mostly used for annealing and oxidation of different samples. Annealing can be done in a nitrogen or argon atmosphere. Recently (Autumn 2013) a bubler has also been installed in the furnace, so it is possible to do both wet and dry oxidations. The maximum temperature of the furnace is 1000 <sup>o</sup>C. | The Noble Furnace is mostly used for annealing and oxidation of different samples. Annealing can be done in a nitrogen or argon atmosphere. Recently (Autumn 2013) a bubler has also been installed in the furnace, so it is possible to do both wet and dry oxidations. The maximum temperature of the furnace is 1000 <sup>o</sup>C. | ||
In the Noble Furnaces more dirty samples with metals and some specific polymers are allowed. Different sample holder are available for wafers and smaller samples. | In the Noble Furnaces more dirty samples with metals and some specific polymers are allowed. Different sample holder are available for wafers and smaller samples (placed on a Si carrier wafer). | ||
The furnace is located in service area 3. | The furnace is located in service area 3. | ||
Please check the cross contamination information in LabManager before you use the furnace. | |||
[[Image:Noble.JPG|thumb|300x300px|Noble furnace. Positioned in service area 3]] | [[Image:Noble.JPG|thumb|300x300px|Noble furnace. Positioned in service area 3]] | ||