The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium.
The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium.


This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed to enter wafers that contain aluminium. Check the cross contamination information in LabManager for more information.  
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace.  


'''The user manual, technical information and contact information can be found in LabManager:'''
'''The user manual, technical information and contact information can be found in LabManager:'''

Revision as of 14:52, 10 January 2014

Feedback to this page: click here

Aluminium Anneal furnace (C4)

Aluminium Anneal furnace (C4). Positioned in cleanroom 2

The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium.

This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom 2. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace.

The user manual, technical information and contact information can be found in LabManager:

Aluminium Anneal furnace (C4)

Process knowledge

Overview of the performance of Aluminium Anneal furnace and some process related parameters

Purpose Annealing
  • Annealing of wafers with aluminium
  • Oxidation of wafers with aluminium
Process parameter range Process Temperature
  • 400-500 oC
Process pressure
  • 1 atm
Gas flows
  • N2: 5 sccm
  • O2: 5 sccm
Substrates Batch size
  • 1-30 100 mm wafers (or 50 mm wafers)
Substrate material allowed
  • Silicon wafers with alluminium.
  • Wafers are allowed enter the furnace after Al lift-off or after Al etch and resist strip in acetone