This is a micrometer-screw.
This is a micrometer-screw.


[[image:Mikrometerskrue_hel_a.JPG|200x200px|right|thumb|The scriber ya da yad]]
[[image:Mikrometerskrue_hel_a.JPG|200x200px|right|thumb|The Thickness measurer in Cleanroom 3 ]]


It measures with an accurracy within a few µm.
It measures with an accurracy within a few µm.

Revision as of 14:12, 9 January 2008

This is a micrometer-screw.

The Thickness measurer in Cleanroom 3

It measures with an accurracy within a few µm. Measure the wafer in the box next to the meter.If ok other wafers can be measured. There is a calibration device by the DEKTAK. It is calibrated at 750µm