SU-8 can be etched by a oxygen plasma with a small amount of SF<sub>6</sub> to remove the antimony present from the photo initiator. | ==Etching of SU-8== | ||
SU-8 can be etched by a oxygen plasma with a small amount of SF<sub>6</sub> to remove the antimony present from the photo initiator. Etching of SU-8 has been developed on the ASE and was tested as a mask less reduction of pattern defined by photo lithography. Two processes are available, a high and a low anisotropic etch for use as etching or thinning of structures. | |||
Revision as of 08:51, 4 November 2013
Etching of SU-8
SU-8 can be etched by a oxygen plasma with a small amount of SF6 to remove the antimony present from the photo initiator. Etching of SU-8 has been developed on the ASE and was tested as a mask less reduction of pattern defined by photo lithography. Two processes are available, a high and a low anisotropic etch for use as etching or thinning of structures.