'''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_cleaning/ | '''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_cleaning/Cleaning_with_Soap_Sonic click here]''' | ||
==Cleaning of wafers or chips that have been out of the cleanroom.== | ==Cleaning of wafers or chips that have been out of the cleanroom.== | ||
Revision as of 16:06, 21 October 2013
Feedback to this page: click here
Cleaning of wafers or chips that have been out of the cleanroom.

The soap sonic is done in a ultrasonic tank placed in the wash bench in the changing room. The soap sonic is DI water with Triton x100 which is free of alkalies. It is used for wafers or chips that has been out of the cleanroom eg. if they have been diced, and you want to bring them in again for measurement or further processing. The soap sonic clean is not enough, you also have to make a piranha clean.
Procedure
You fill up the tank with DI water and add 20 - 30 drops of Triton x100 soap. Start the sonic and leave for 10 min. rinse, dry and continue with piranha.