Specific Process Knowledge/Thermal Process/C3 Anneal-bond furnace: Difference between revisions
Appearance
No edit summary |
|||
| Line 4: | Line 4: | ||
[[Image:C3.JPG|thumb|300x300px|C3 Anneal-bond furnace. Positioned in cleanroom 2]] | [[Image:C3.JPG|thumb|300x300px|C3 Anneal-bond furnace. Positioned in cleanroom 2]] | ||
The Anneal-bond furnace (C3) is a Tempress horizontal furnace for oxidation and annealing of (bonded) silicon wafers. | The Anneal-bond furnace (C3) is a Tempress horizontal furnace for oxidation and annealing of new and processed (bonded) silicon wafers. | ||
This furnace is the third furnace tube in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed | This furnace is the third furnace tube in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed oxidize and anneale wafers without doing a RCA clean first. Also bonded wafers comming directly from the EVG NIL (assuming they were very clean when entering EVG NIL and not contain any metal). Check the cross contamination information in LabManager can enter the furnace. Check the cross contamination information in LabManager. | ||
'''The user manual, technical information and contact information can be found in LabManager:''' | '''The user manual, technical information and contact information can be found in LabManager:''' | ||
Revision as of 15:11, 9 January 2014
Feedback to this page: click here
Anneal-bond furnace (C3)
The Anneal-bond furnace (C3) is a Tempress horizontal furnace for oxidation and annealing of new and processed (bonded) silicon wafers.
This furnace is the third furnace tube in the furnace C-stack positioned in cleanroom 2. In this furnace it is allowed oxidize and anneale wafers without doing a RCA clean first. Also bonded wafers comming directly from the EVG NIL (assuming they were very clean when entering EVG NIL and not contain any metal). Check the cross contamination information in LabManager can enter the furnace. Check the cross contamination information in LabManager.
The user manual, technical information and contact information can be found in LabManager:
Process knowledge
| Purpose | Oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|