Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of TiW: Difference between revisions

From LabAdviser
BGE (talk | contribs)
New page: Deposition of TiW alloy can take place in the Wordentec.
 
Kn (talk | contribs)
No edit summary
Line 1: Line 1:
Deposition of TiW alloy can take place in the Wordentec.
Deposition of TiW alloy can take place in the Wordentec.
This is done by a sputtering process, process parameters (argon pressure and effect) can be varied, and the deposition rate and surface roughness may change with these settings.

Revision as of 12:39, 14 August 2008

Deposition of TiW alloy can take place in the Wordentec.

This is done by a sputtering process, process parameters (argon pressure and effect) can be varied, and the deposition rate and surface roughness may change with these settings.