Jump to content

Specific Process Knowledge/Lithography/Coaters: Difference between revisions

Elkh (talk | contribs)
Elkh (talk | contribs)
Line 366: Line 366:
'''The user manual, user APV, and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=43 LabManager]'''
'''The user manual, user APV, and contact information can be found in [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=43 LabManager]'''


<br clear="all" />
=== Equipment performance and process related parameters ===
{| border="2" cellspacing="0" cellpadding="2"
!style="background:silver; color:black;" align="center" width="60"|Purpose
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black"|
*Spin coating and soft baking UV sensative resists
*Spin coating SU8 resists
|-
!style="background:silver; color:black;" align="center" width="60"|Resist
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black" align="center"|
* AZ5214E permanent line
* AZ4562 manual dispense
* SU8 resists manual dispense
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="1"|Performance
|style="background:LightGrey; color:black"|Coating thickness
|style="background:WhiteSmoke; color:black" align="center"|
* AZ5214E 1-4,2 µm
* AZ4526 6,2-10 µm
* SU8 resits 0,1-100 µm
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameters
|style="background:LightGrey; color:black"|Spin speed
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
100 - 5000 rpm
|-
|style="background:LightGrey; color:black"|Spin acceleration
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
100 - 5000 rpm/s
|-
|style="background:LightGrey; color:black"|Hotplate temperature
|style="background:WhiteSmoke; color:black" align="center"|
* changeable temperature from 20 to 200
* SU8 must be bake out on SU8 dedicated hotplates
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates
|style="background:LightGrey; color:black"|Substrate size
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
* 50 mm wafers
* 100 mm wafers
* 150 mm wafers
|-
| style="background:LightGrey; color:black"|Allowed materials
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
All cleanroom materials except III-V materials
|-
|style="background:LightGrey; color:black"|Batch
|style="background:WhiteSmoke; color:black" align="center" colspan="2"|
1
|-
|}


<br clear="all" />
<br clear="all" />