==Wet etching of Chromium==
==Wet etching of Chromium==
[[Image:Stinkskab RR2.jpg|300x300px|thumb|Fume hood in cleanroom 2. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]
[[Image:Stinkskab RR2.jpg|300x300px|thumb|Fume hood in cleanroom B-1. <br />Wet Etch of Chromium can take place in a beaker in this fume hood]]
Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. You can see the APV [http://labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here].
Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom B-1 or D-3. You can see the APV [http://labmanager.danchip.dtu.dk/d4Show.php?id=2479&mach=146 here].


We have two solutions for this:
We have two solutions for this: