Jump to content

Specific Process Knowledge/Etch/Wet Titanium Etch: Difference between revisions

Kabi (talk | contribs)
No edit summary
Kabi (talk | contribs)
Line 79: Line 79:


|-style="background:LightGrey; color:black"
|-style="background:LightGrey; color:black"
!Etch bath
!Size of substrate
|Beaker or PP-etch bath in the fume hood in cleanroom 2.
|Any size and number that can go inside the beaker in use.  
|Beaker
|Any size and number that can go inside the beaker in use.
|-
|-